SWC Forums
Pull up a chair...let's talk fishing.
Last year I had a hawse pipe installed on my forward deck. It did not work out well, so I had a hatch fabricated for my anchor rode. Installed it last week, tried to remove the hawse pipe. NO WAY it was sealed with 5200. Went to another site and asked about removing 5200. I was given 2 options. Heat Gun or DeBond. Since I did not have a heat gun and was reading about the drawbacks of it I decided to go the DeBond route. Ordered a 4 ounce spray can. Removed the screws sprayed in the holes. Then spayed it around the edge of the hawse pipe. After about 2 minutes I was able to get a metal scraper under it and it lifted right up. Used a little more to clean the excess off the deck. This stuff is absolutely amazing it ate right through the 5200. Just thought I would share.
thanks for the info Barry, I was wandering how I was gonna get that stuff off
that is the first time I have heard of anything working with 5200, thanks for the info.
Picture of your hatch? I'm about to install a hawse and sure would like an alternative ... :chin:
Thanks for that info
If any one needs this stuff here is a link.
http://www.debondcorporation.com/products/marine-formula
I didn't think there was anything that would take 5200 off other than abrasives, thanks for the info.
I looked at the MSDS and it appears the primary ingredient is a member of the Glycol family. We use a glycol ether/peroxide mixture to soften thick film polyurethane coatings ...... Hmmmmmmm
Is it expensive?
I bought the 4 ounce spray. Like $18.00 + shipping. The 12 ounce I thinks about $28.00